Mechanical behavior of recycled PP compounds : tensile, bending and creep tests

Publication Type:

Journal Article

Authors:

Rogueda-Berriet, C.; Bahlouli, N.; Pessey, D.

Source:

Journal of Engineering Materials and Technology, Volume 3, Number 030907, p.133 (2011)

URL:

http://hal.archives-ouvertes.fr/hal-00662581